COPPER FOIL FREE FROM GENERATION OF WRINKLE, ELECTRODE COMPRISNG THE SAME, SECONDARY BATTERY COMPRISING THE SAME AND METHOD FOR MANUFACTURING THE SAME

机译:铜箔没有产生皱纹,电极特征相同,二次电池包括相同的和制造方法

摘要

An embodiment of the present invention, a copper layer having a matte surface and a shiny surface; And a rust prevention film disposed on the copper layer, and has a residual stress of 0.5 to 25 Mpa based on an absolute value, and the copper layer includes: copper; And carbon (C); In the copper layer, the content of the carbon (C) is 2 to 20 ppm, and the copper layer is a (111) plane containing crystalline particles, (200 ) Plane, (220) plane, and (311) plane, among the sum of diffraction intensity of the (111) plane, the (200) plane, the (220) plane, and the (311) plane, The ratio occupied by the diffraction intensity is 10 to 40%, and the crystalline particles of the (220) plane at room temperature provide a copper foil having an average particle size of 70 to 120 nm.
机译:本发明的一个实施方案,具有哑光表面和闪亮表面的铜层;设置在铜层上的防锈膜,并且基于绝对值的剩余应力为0.5至25MPa,铜层包括:铜;和碳(c);在铜层中,碳(C)的含量为2至20ppm,铜层是含有晶体颗粒的(111)平面,(200)平面,(220)平面和(311)平面(111)平面,(200)平面,(220)平面和(311)平面的衍射强度之和,衍射强度占据的比率为10〜40%,以及晶体颗粒(220)在室温下平面提供平均粒径为70至120nm的铜箔。

著录项

  • 公开/公告号KR20210062204A

    专利类型

  • 公开/公告日2021-05-31

    原文格式PDF

  • 申请/专利权人 에스케이넥실리스 주식회사;

    申请/专利号KR1020190150119

  • 发明设计人 김선화;이안나;김승민;

    申请日2019-11-21

  • 分类号C25D1/04;C23C22/24;C23C28;C25D3/38;C25D5/48;H01M4/66;

  • 国家 KR

  • 入库时间 2024-06-14 21:36:56

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号