Asphalt-rubber was tested with conventional and non-conventional methods to begin development of testing methods for specification purposes and to find methods for studying the reaction between asphalt and reclaimed crumb rubber. A single asphalt-rubber formulation consisting of 75 percent AR-1000 asphalt and 25 percent crumb rubber from automobile tire treads (sized from No. 16 to No. 25) was used. Dependent variables included ring and ball softening point, absolute viscosity by capillary viscometer at 140 F (60 C), ductility and force-ductility at 39.2 F (4 C), elastic rebound, and low temperature viscosity with the Schweyer rheometer at 39.2 F (4 C). Recommendations are made for new tests, modifications of conventional tests and improved laboratory mixing and formulation techniques.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号