Zr-riched lead zirconate titanate, Pb(Zr0.95Ti0.05)O-3 (PZT 95/5) powders were prepared using lead acetate, zirconium oxynitrate, and titanium sulfate by aqueous Pechini method. The chelation behaviors of metallic ions and citric acid were investigated and the development of the phase formation of perovskite structure was detected. PZT 95/5 powders were obtained directly from the as-synthesized gels by one-step pyrolysis process at 450 degrees C for 10 h. Perovskite phase was formed at about 450 degrees C and no distinct intermediates were obtained. There were some carbonates as impurities but they did not affect the formation of the complete perovskite phase of PZT 95/5 ceramics after sintering at 1,100-1,150 degrees C for 2 h. The decomposition of few organic residues among the one-step pyrolyzed powders could form uniform porous structure and the formation mechanism of porous ceramics was also presented.
机译:利用醋酸铅,氧氮化锆和硫酸钛,通过水溶Pechini法制备了富Zr的钛酸锆钛酸铅,Pb(Zr0.95Ti0.05)O-3(PZT 95/5)粉末。研究了金属离子与柠檬酸的螯合行为,并检测了钙钛矿结构相形成的发展。 PZT 95/5粉末是从合成后的凝胶中通过一步一步热解过程在450摄氏度,10小时的条件下直接获得的。钙钛矿相在约450℃形成,没有得到明显的中间体。有一些碳酸盐作为杂质,但在1,100-1,150摄氏度下烧结2小时后,它们并不影响PZT 95/5陶瓷的完整钙钛矿相的形成。一步热解粉中很少的有机残留物分解可以形成均匀的多孔结构,并提出了多孔陶瓷的形成机理。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号