A spent processing catalyst from an Iranian oil refinery was initially characterized physically and chemically. Acidithiobacillus ferrooxidans and Acidithiobacillus thiooxidans were used to mobilize Al, Co, Mo and Ni from the spent catalysts under optimized conditions in batch cultures. The characteristics of the bioleach solution (pH, Eh, cell concentration and Fe(II)/Fe(III) concentration) were determined along with the concentration of metal values extracted from the catalyst. The results showed that after bioleaching using A. ferrooxidans in the presence of ferrous sulfate, maximum extractions of 63% Al, 96% Co, 84% Mo and 99% Ni were achieved after 30 days at pH 1.8–2.0. However, the highest extractions using A. thiooxidans in the presence of sulfur were 2.4% Al, 83% Co, 95% Mo and 16% Ni after 30 days at pH 3.9–4.4. The recovery of these metals decreases the environmental impact of the waste catalyst and the recycled product can be further used for industrial purposes.
机译:最初从物理和化学上对伊朗炼油厂的废催化剂进行了表征。酸性氧化硫杆菌铁氧体和酸性氧化硫杆菌素用于在分批培养中的最佳条件下从废催化剂中动员Al,Co,Mo和Ni。确定了生物浸出溶液的特性(pH,Eh,细胞浓度和Fe(II)/ Fe(III)浓度)以及从催化剂中提取的金属值的浓度。结果表明,在硫酸亚铁存在下使用A. ferrooxidans进行生物浸出后,在pH 1.8-2.0的条件下30天后,最大提取量为63%Al,96%Co,84%Mo和99%Ni。但是,在pH值为3.9-4.4的30天后,在硫磺存在下,使用硫代农杆菌的最高提取量为2.4%Al,83%Co,95%Mo和16%Ni。这些金属的回收减少了废催化剂对环境的影响,回收的产品可进一步用于工业目的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号