Porous Titanium Scaffolds were produced by using a rapid prototyping technique. These scaffolds were either coated or not with a calcium phosphate coating via an eletrodeposition method. Rat bone marrow mesenchymal stem cells were cultured on the scaffolds at a density of 10~6 cells/scaffold for a period of 3 days. Cell proliferation was measured by using the Alamar Blue assay. The scaffolds were observed by SEM and polarized light microscopy. Constructs were then implanted subcutaneously for 4 weeks in syngenic rats. Cells proliferated well after seeding. After subcutaneous implantation, histology and SEM revealed the presence of uniform coatings as well as Ca and P deposits in the non-coated scaffolds suggesting mineralization.