We introduce low-loss amorphous titanium dioxide (TiO$_{2}$ ) strip waveguides with sub-wavelength dimensions. The waveguides were fabricated by the combination of atomic layer deposition (ALD), electron beam lithography (EBL), and reactive ion etching (RIE). Propagation losses of the strip waveguides were found to be as low as 5.0 dB/cm at 1.55 $mu$ m wavelength. Those propagation losses are mostly due to the sidewall roughness of the waveguides that is caused by the lithography process. The propagation losses were further reduced by deposition, on the fabricated strip waveguides, of an additional layer of TiO$_{2}$ made by using ALD. A supplementary layer of TiO$_{2}$ with a thickness of 30 nm reduced the measured propagation losses from 5.0 $pm$ 0.5 dB/cm to 2.4 $pm$ 0.2 dB/cm at 1.55 $mu$m wavelength. It is due to the fact that, after the redeposition process, the initial waveguide sidewall, i.e., the TiO$_{2}$ /air interface, is virtually removed and the new sidewall has a reduced roughness.
机译:我们介绍了具有亚波长尺寸的低损耗非晶态二氧化钛(TiO $ _ {2} $)条形波导。通过结合原子层沉积(ALD),电子束光刻(EBL)和反应离子刻蚀(RIE)来制造波导。发现在1.55μm的波长下,条形波导的传播损耗低至5.0dB / cm。这些传播损耗主要是由于光刻工艺导致的波导侧壁粗糙度。通过在制造的带状波导上沉积使用ALD制成的TiO $ _ {2} $的附加层,可以进一步降低传播损耗。厚度为30 nm的TiO $ {2} $补充层将所测得的传播损耗在波长为1.55μm的情况下从5.0 $ pm $ 0.5 dB / cm减小到2.4 $ pm $ 0.2 dB / cm。由于这样的事实,在重新沉积过程之后,实际上去除了初始波导侧壁,即TiO 2空气界面,并且新的侧壁具有降低的粗糙度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号