Pulsed laser deposition films from a Ba_2FeMoO_6 target onto SrTiO_3[001]: Chemical and magnetic inhomogeneity

机译:从Ba_2FeMoO_6靶到SrTiO_3的脉冲激光沉积膜[001]:化学和磁性不均匀性

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Pulsed laser deposition films from Ba2FeMoO6 (BFMO) targets onto SrTiO3[001] (STO) substrates have been reported previously to have non-zero magnetism at 300 K, a majority of magnetic ordering at 240 K that is less than the 370 K ordering temperature of polycrystalline BFMO, and suppressed saturation magnetization compared to polycrystalline BFMO. To interrogate these previously reported observations of BFMO on STO, we have used a combination of x-ray diffraction, atomic force microscopy, x-ray and neutron reflectivity, and x-ray photoelectron spectroscopy that shows inhomogeneities. The present results show off-stoichiometry on the A-site by incorporation of Sr from the substrate and on the B-site to have %Fe/%Mo 1 by evolution of BaMoO4. There is an enhanced ordering temperature and magnetic response nearer to the SrTiO3 interface compared to the air interface. Depth dependent strain and microstructure are needed to explain the magnetic response. Holistic considerations and implications are also discussed. Published by AIP Publishing.
机译:先前已经报道了从Ba2FeMoO6(BFMO)靶材到SrTiO3 [001](STO)衬底上的脉冲激光沉积膜在300 K时具有非零磁性,大多数在240 K时的磁性有序,低于370 K的有序温度。与多晶BFMO相比,多晶BFMO具有更好的抑制性能,并且抑制了饱和磁化强度。为了询问这些先前报道的BFMO在STO上的观察结果,我们结合使用了X射线衍射,原子力显微镜,X射线和中子反射率以及显示不均匀性的X射线光电子能谱。目前的结果表明,通过掺入来自底物的Sr,在A位上的化学计量不正确;而在Ba位上,由于BaMoO4的析出,%Fe /%Mo> 1时,化学计量不正确。与空气界面相比,靠近SrTiO3界面的订购温度和磁响应增强。需要深度依赖的应变和微观结构来解释磁响应。还讨论了整体考虑和含义。由AIP Publishing发布。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号