Development of Blood Compatible Alpha-lipoic acid Coated Stent with a Good Adhesive by Low Temperature Plasma Polymerization

机译:通过低温等离子体聚合,涂有良好粘合剂的血液相容性α-脂质酸涂覆支架

获取原文

摘要

Neointimal hyperplasia is a main cause for in-stent restenosis after stent-implantation and is triggered by inflammatory response to foreign materials. It can be inhibited if the stent is modified to have good blood compatibility by coating drug compounds. Low temperature plasma polymerization of 1,2-diaminocyclohexane was performed to prepare more adhesive polymeric thin film onto the metallic stent. Then, the chemical grafting of a-lipoic acid (ALA) was carried out to improve blood compatibility of stent. Drugs containing carboxylic groups can be chemically grafted through the formation of amide bond in the presence of 1-ethyl-3-(3-dimethylaminopropyl) carbodiimide methiodide onto the DACH deposited stent surface. ALA grafted film showed good mechanical stability and blood compatibility.
机译:内部增生是支架植入后支架再狭窄的主要原因,并通过对异物的炎症反应引发。如果通过涂覆药物化合物,可以抑制支架以具有良好的血液相容性,可以抑制它。进行1,2-二氨基环己烷的低温等离子体聚合以制备更多的粘合剂聚合物薄膜在金属支架上。然后,进行α-硫辛酸(ALA)的化学接枝以改善支架的血液相容性。含有羧基的药物可以通过在1-乙基-3-(3-二甲基氨基丙基)碳二亚胺甲基碘化物上的酰胺键在达氏沉积的支架表面上形成酰胺键来化学接枝。 ALA接枝膜显示出良好的机械稳定性和血液相容性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号