首页> 外国专利> A procedure for the utilization of residual material of mines of hulla. (Machine-translation by Google Translate, not legally binding)

A procedure for the utilization of residual material of mines of hulla. (Machine-translation by Google Translate, not legally binding)

机译:一种利用赫拉矿剩余材料的程序。 (通过Google翻译进行机器翻译,没有法律约束力)

摘要

A method for the use of coal mine residual material containing coal, which comprises passing through a hydrocyclone a slurry in water of crushed waste material having a grain size no greater than 20 mm and of which at least 40 mm. % by weight has a grain size of not more than 1 mm with a grain size distribution of less than 1 snm of: 0.0 - 0.05 mm between 10 and 30%; 0.05 - 0.5 mm between 20 and 50%; 0.5 - 1 mm between 30 and 70%; the density of the suspension being adjusted by addition of water to leave it within the range of 1.22 to 1.45 kg/liter, to separate said residual material into a fraction, rich in coal and a poor fraction in coal. (Machine-translation by Google Translate, not legally binding)
机译:一种使用含煤的煤矿残余物的方法,该方法包括使水流通过水力旋流器,使粉碎后的废料的水中的浆液的粒度不大于20mm,其中至少40mm。重量%具有不大于1mm的晶粒尺寸,且小于1snm的晶粒尺寸分布为:0.0-0.05mm,在10%至30%之间;优选地,在0.03mm至3mm之间。 0.05-0.5毫米,介于20%和50%之间; 0.5-1毫米,介于30%和70%之间;通过加入水来调节悬浮液的密度,使之保持在1.22-1.45kg /升的范围内,以将所述残余物质分离成富含煤的部分和富含煤的部分。 (通过Google翻译进行机器翻译,没有法律约束力)

著录项

  • 公开/公告号ES411606A3

    专利类型

  • 公开/公告日1976-01-01

    原文格式PDF

  • 申请/专利权人 NIKEX NEHEZIPARI KULKERESKEDELMI VALLALAT;

    申请/专利号ES19730411606

  • 发明设计人

    申请日1973-02-14

  • 分类号F23G;C04B;

  • 国家 ES

  • 入库时间 2022-08-23 02:30:20