METHOD FOR REGENERATING ETCHING POWER OF ETCHING SOLUTION FOR COPPER OR COPPER ALLOY

机译:铜或铜合金的蚀刻液的蚀刻力的再生方法

摘要

PURPOSE:To restore and regenerate easily and surely etching power by blowing air contg. oxygen in a high concn. to an etching soln. in which cuprous ion is formed by etching thereby converting the same to cupric ion. CONSTITUTION:Ordinary air (a) is passed through a filter F1 and is fed to a nitrogen adsorber 23 after the air is energized by a compressor 22. Nitrogen is removed from the air in said device to create the air (a') of high oxygen concn. contg. =40vol% oxygen which is then stored in a storage tank 24. The air is passed through a filter F2 and the concn. and flow rate thereof are measured by an oxygen densitometer 2 and a flowmeter 26 and is blown through a humidifier 27 and an air blowing pipe 20 into the etching soln. The cuprous ion formed in the etching soln. is thus regenerated to cupric ion.
机译:目的:通过吹气来轻松,可靠地恢复和再生腐蚀力。高浓度氧气。蚀刻液。其中通过蚀刻形成亚铜离子,从而将其转化为铜离子。组成:普通空气(a)经过过滤器F1,并由压缩机22供电后送入氮气吸附器23。氮气从所述装置中的空气中去除,从而产生高浓度的空气(a')。氧气浓度续> = 40vol%的氧气,然后将其存储在存储箱24中。空气通过过滤器F2和浓缩液。其流量由氧气密度计2和流量计26测量,并通过加湿器27和吹气管20吹入蚀刻液中。在蚀刻液中形成亚铜离子。因此被再生为铜离子。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号