A process for producing a sulfur sorbent composition in a mixer having a mixer paddle an energy supply is disclosed which includes hydrating an alkaline earth metal oxide in an aqueous solution containing a promoting additive selected from a group consisting of urea and mixtures of urea with a water soluble iron salt under high intensity mixing conditions with the mixer wherein the mixer is operated at a mixer paddle tip velocity of at least 500 ft/min and a mixer energy input of at least 3.5 kW-h per ton of sorbent so as to produce a sulfur sorbent composition having the following physical and chemical properties: alkaline earth metal (wt.%)--40-52, molar ratio of promoting additive to alkaline earth metal--0.001-0.2, bulk density (g/ml)--0.35-0.75, surface area (m.sup.2 /g)--5-25, pore volume (cc/g)--0.05-0.14 and mean particle size (&mgr;m)-- 4.
机译:公开了一种在具有能量供应的混合器桨叶的混合器中生产硫吸附剂组合物的方法,该方法包括在含有促进剂的水溶液中水合碱土金属氧化物,所述促进剂选自尿素和尿素与水的混合物。可溶性铁盐在混合机的高强度混合条件下,其中混合机以至少500 ft / min的混合器桨叶尖端速度和每吨吸附剂至少3.5 kW-h的混合器能量输入运行,以产生具有以下物理和化学性质的硫吸附剂组合物:碱土金属(wt。%)-40-52,促进添加剂与碱土金属的摩尔比-0.001-0.2,堆积密度(g / ml)-0.35 -0.75,表面积(m.sup.2 / g)-5-25,孔容(cc / g)-0.05-0.14和平均粒径(μm)-4。

著录项

  • 公开/公告号PL299243A1

    专利类型

  • 公开/公告日1993-12-13

    原文格式PDF

  • 申请/专利权人 INTEVEP SA;

    申请/专利号PL19930299243

  • 申请日1993-06-08

  • 分类号B01J20/00;B01D53/02;

  • 国家 PL

  • 入库时间 2022-08-22 04:44:46

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号