Method for processing sulfur-containing residues into hardened granules, manufacturing a cementless mortar and a building block composed of such granules and mortar.

机译:将含硫残留物加工成硬化颗粒的方法,制造无水泥砂浆和由这种颗粒和砂浆组成的结构块。

摘要

In a method of processing sulphur-contaning residue and fly ash into cured granules, the residue is mixed with fly ash and water to make a mixture, the mixture is granulated and the granules are heated to effect curing. In the granulatable mixture, the amount of fly ash is not more than 20% by weight relative to the total amount of said fly ash and the residue. A cementless mortar is made from fly ash, by mixing fly ash with [chalk] lime and other components to form a mixture containing by weight (i) fly ash : maximum 85% (ii) optionally, an amount of sand not exceeding the amount of fly ash (iii) (chalk) lime : 6 - 12% (iv) other components : remainder, and maintaining the pH of the mixture in the range 12.8 - 13.4. This mortar and the granules are combined to make a building block.
机译:在将含硫残余物和粉煤灰加工成固化颗粒的方法中,将残余物与粉煤灰和水混合以形成混合物,将混合物制粒并将颗粒加热以进行固化。在可粒化的混合物中,粉煤灰的量相对于所述粉煤灰和残余物的总量不超过20重量%。无水泥砂浆是由粉煤灰制成的,方法是将粉煤灰与[粉笔]石灰和其他成分混合,形成一种混合物,其中含有以下混合物:(i)粉煤灰:按重量计:最大85%(ii)砂的含量不超过其含量粉煤灰(iii)(白垩)石灰:6-12%(iv)其他组分:剩余物,并将混合物的pH值保持在12.8-13.4的范围内。将该砂浆和颗粒结合在一起以构成构件。

著录项

  • 公开/公告号NL9301309A

    专利类型

  • 公开/公告日1995-02-16

    原文格式PDF

  • 申请/专利号NL19930001309

  • 发明设计人

    申请日1993-07-26

  • 分类号C04B18/02;C04B18/06;

  • 国家 NL

  • 入库时间 2022-08-22 04:19:02

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号