PROBLEM TO BE SOLVED: To provide a method for producing a Bi4Ti3O12 ferroelectric for a dense sintered compact by a simple process. ;SOLUTION: The designated amounts of TiO2 powder and Bi2O3 powder as raw materials are weighed, blended to obtain calcined powder, which is then compacted. The compacted body is filled in a carbon die together with reduction preventing powder, which is then sintered while plasma is discharged by a constant heating speed sintering method to sinter a sample by heating to 800-1,000°C at a constant speed under pressure and holding for a prescribed time or a constant electric current sintering method to sinter a sample while supplying a constant electric current under pressure until 800-900°C to produce the sintered compact having 95% relative density with good reproducibility.;COPYRIGHT: (C)2000,JPO
机译:要解决的问题:提供一种通过简单的方法生产用于致密烧结体的Bi4Ti3O12铁电体的方法。 ;解决方案:称量指定数量的TiO2粉和Bi2O3粉为原料,混合后得到煅烧粉,然后压实。将压实体与防还原粉末一起填充到碳模中,然后将其烧结,同时通过恒定加热速度烧结法排出等离子体,以在恒定压力下以恒定速度加热至800-1,000°C并保持并烧结样品。规定的时间或采用恒定电流烧结法烧结样品,同时在压力下提供恒定电流直至800-900°C,以生产相对密度为95%的烧结体并具有良好的重现性。;版权:(C)2000 ,日本特许厅

著录项

  • 公开/公告号JP2000302545A

    专利类型

  • 公开/公告日2000-10-31

    原文格式PDF

  • 申请/专利权人 SUMITOMO SPECIAL METALS CO LTD;

    申请/专利号JP19990113820

  • 发明设计人 SHIMADA SHIRO;TAKAHASHI JUNICHI;

    申请日1999-04-21

  • 分类号C04B35/46;H01B3/12;

  • 国家 JP

  • 入库时间 2022-08-22 02:01:27

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号