首页> 外国专利> MOLDING MATERIAL CONTAINING POLYAMINE/POLYAMIDE COPOLYMER, ITS USE AND ARTICLE CONTAINING THE MOLDING MATERIAL

MOLDING MATERIAL CONTAINING POLYAMINE/POLYAMIDE COPOLYMER, ITS USE AND ARTICLE CONTAINING THE MOLDING MATERIAL

机译:包含聚酰胺/聚酰胺共聚物的模塑材料,其用途和包含模塑材料的物品

摘要

PROBLEM TO BE SOLVED: To produce a molding material which has better cuttablity and blow moldability than those of conventional polyamide molding materials, and has a high melt rigidity.;SOLUTION: The molding material comprises a polyamine/polyamide copolymer to be produced by using (a) 0.05-2.5 mass% (based on the polyamine/ polyamide copolymer) polyamine having at least 4 nitrogen atoms and (b) a polyamide-forming monomer to be selected from an equimolar compound of a lactam, an ω-aminocarboxylic acid and/or a diamine and a dicarboxylic acid, and meets the conditions that the viscosity at -250°C is at least 5,000 Pa.s and the shear rate is 0.1 1/s; and the viscosity ratio at -250°C is at least 7 (in this instance the melt viscosities at shear rates of 0.1 1/s and 100 1/s being compared with each other).;COPYRIGHT: (C)2002,JPO
机译:解决的问题:要生产一种比传统的聚酰胺模塑材料具有更好的可切割性和吹塑性,并且具有高熔体刚度的模塑材料;解决方案:该模塑材料包含一种聚胺/聚酰胺共聚物,该共聚物可以通过使用( a)0.05-2.5质量%(基于聚胺/聚酰胺共聚物)具有至少4个氮原子的聚胺,和(b)选自内酰胺,ω-氨基羧酸和/或二胺和二羧酸,并满足以下条件:在-250℃下的粘度为至少5,000Pa.s,剪切速率为0.1 1 / s; ;和-250℃时的粘度比至少为7(在这种情况下,将剪切速率为0.1 1 / s和100 1 / s时的熔体粘度进行比较)。版权所有:(C)2002,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号