PURPOSE: To provide an Fe-Ni-Co based alloy which combines high strength and excellent magnetic properties, and has a low thermal expansion coefficient. CONSTITUTION: The Fe-Ni-Co based alloy thin strip for a shadow mask having high strength and excellent magnetic properties, and maintaining a low thermal expansion coefficient comprises 30 to 35% Ni, 2 to 6% Co, 0.1 to 0.4% Nb and 0.2 to 0.5% Mn, and the balance Fe with inevitable impurities, and in the inevitable impurities, the content of C is controlled to =0.005%, S to =0.002% and N to =0.005%. The crystal grain size before etching piercing is 7.0 to 10.0 by a crystal grain size number prescribed in JISG0551, and the total content of precipitates and inclusions of 0.2 to 5 μm is 0.5 to 1.5 μg/mm¬3.
展开▼
机译:目的:提供一种具有高强度和优异的磁性能,并且具有低热膨胀系数的Fe-Ni-Co基合金。组成:用于荫罩的Fe-Ni-Co基合金薄带,具有高强度和优异的磁性能,并保持低的热膨胀系数,包括30%至35%的Ni,2%至6%的Co,0.1%至0.4%的Nb和Mn为0.2〜0.5%,余量的Fe为不可避免的杂质,在不可避免的杂质中,将C的含量控制为≤0.005%,S为≤0.002%,N为≤0.005%。根据JIS G0551中规定的晶粒尺寸号,蚀刻穿孔之前的晶粒尺寸为7.0至10.0,并且0.2至5μm的析出物和夹杂物的总含量为0.5至1.5μg/ mm 3。
展开▼