FIELD: electrical engineering.;SUBSTANCE: storage battery is charged with regulated asymmetric current, proportion of discharge-to-charge pulse amplitudes being 3-4 and numeric values of charge pulse amplitudes equal to 0.3-0.5 of rated capacity at charge pulse length of 220 20 ms and discharge pulse length of 15 5 ms with intervals between them of 0-2 ms; charging process lasts until voltage across battery is brought to threshold value specified by Standard Specifications or by relevant operating instructions, or until charge capacity amounting to 120-150% of rated value is attained. Battery voltage is measured during interval between charge and discharge current pulses.;EFFECT: reduced time taken for battery formation and recovery, reduced gas emission.;1 cl
机译:领域:电气工程;研究对象:用规定的不对称电流对蓄电池充电,充放电脉冲幅度为3-4时,充放电脉冲幅度的比例为3-4,并且充电脉冲幅度的数值等于额定容量的0.3-0.5。 220 20 ms,放电脉冲长度为15 5 ms,它们之间的间隔为0-2 ms;充电过程持续进行,直到电池两端的电压达到标准规范或相关操作说明指定的阈值为止,或者直至达到额定容量的120-150%。在充电和放电电流脉冲之间的间隔内测量电池电压;效果:减少了电池形成和恢复所需的时间,减少了气体排放; 1 cl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号