METHOD FOR HIGH-SPEED FORMATION AND RECOVERY OF SEALED NICKEL-CADMIUM STORAGE BATTERIES BY CHARGING THEM WITH ASYMMETRIC CURRENT

机译:通过不对称电流对密封的镍镉存储电池进行高速形成和恢复的方法

摘要

FIELD: electrical engineering; reducing battery formation and recovery time.;SUBSTANCE: proposed storage battery is charged with regulated asymmetric current, proportion of discharge to charge pulse amplitudes being 0.3-0.8 of rated capacity at charge pulse amplitudes numerically equal to 0.3-0.8 of rated capacity with charge pulse length of 220 20 ms and discharge pulse length of 15 5 ms, intervals between them being 0-2 ms; battery is charged until threshold value specified by Standard Specifications or relevant operating instructions is attained or until voltage across battery reduces by 15 5 mV per cell after it crosses maximal value. Voltage across battery is measured during intervals between charge and discharge current pulses.;EFFECT: reduced time taken to place battery in operation upon long-time storage.;1 cl
机译:领域:电气工程;实质:拟议的蓄电池以稳定的不对称电流充电,在充电脉冲幅度数值等于带充电脉冲的额定容量的0.3-0.8的情况下,放电与充电脉冲幅度的比例为额定容量的0.3-0.8长度为220 20 ms,放电脉冲长度为15 5 ms,它们之间的间隔为0-2 ms;电池充电直到达到标准规格或相关操作说明指定的阈值,或者直到电池两端的电压超过最大值后降低15 5 mV。在充电和放电电流脉冲之间的时间间隔内测量电池两端的电压;效果:长时间存放可减少电池投入使用的时间; 1 cl

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号