A manufacturing method of a multicomponent bismuth molybdate catalyst for manufacturing 1,3-butadiene is provided to manufactured with a corecipitation method on a co-precipitated solution of which a pH is controlled. A manufacturing method of a multicomponent bismuth molybdate catalyst comprises steps of: preparing a first solution including a precursor of a metallic component of divalent cation, a precursor of a metallic component of 3-valent cation and a bismuth precursor; preparing a second solution dissolving a molybdenum precursor; injecting the first solution into the second solution, co-precipitating the first solution and the second solution, dipping a basic solution of 1~3 molarity into a co-precipitated solution and controlling the co-precipitated solution to pH of 6 ~ 8; obtaining a solid-component by removing moisture after mixing the co-precipitated solution of which a pH is controlled for 1~2 hours; and heat-treating the solid-component to 400~600‹C after drying the solid-component at 20 ~300‹C.
机译:本发明提供一种用于制造1,3-丁二烯的多组分钼酸铋催化剂的制造方法,其是通过共沉淀法在pH被控制的共沉淀溶液上制造的。一种多组分钼酸铋催化剂的制备方法,包括以下步骤:制备第一溶液,所述第二溶液包含二价阳离子的金属组分的前体,3-价阳离子的金属组分的前体和铋前体。制备溶解钼前体的第二溶液;将第一溶液注入第二溶液中,使第一溶液与第二溶液共沉淀,将摩尔浓度为1〜3的碱性溶液浸入共沉淀溶液中,并将共沉淀溶液的pH控制为6〜8。将pH值控制好的共沉淀溶液混合1〜2小时后,除去水分,得到固体成分。在20〜300℃下干燥后,将固体成分加热至400〜600℃。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号