Disclosed is a bound phosphorus-modified zeolite catalyst. Zeolite is treated with a phosphorus compound to form the phosphorus-treated zeolite. Binder material is treated with a mineral acid prior to being bound with the phosphorus-modified zeolite. The binder material includes inorganic oxide materials, such as alumina, clay, aluminum phosphate and silica- alumina, in particular, a binder of alumina or clay or their combinations. The mineral acid includes hydrochloric acid, nitric acid, phosphoric acid or sulfuric acid. The phosphorus- treated zeolite is combined with the acid-treated inorganic oxide binder material to form a zeolite-binder mixture. Water is added to form an extrudable paste which maybe shaped and is heated to a temperature of about 4000C or higher to form a bound phosphorus-modified zeolite catalyst. For aromatic alkylation, the bound phosphorus-modified zeolite catalyst is contacted with an aromatic alkylation feed of an aromatic compound and an alkylating agent under reaction conditions suitable for aromatic alkylation.
机译:公开了一种键合的磷改性的沸石催化剂。用磷化合物处理沸石以形成经磷处理的沸石。在与磷改性的沸石结合之前,将粘合剂材料用无机酸处理。粘合剂材料包括无机氧化物材料,例如氧化铝,粘土,磷酸铝和二氧化硅-氧化铝,特别是氧化铝或粘土的粘合剂或它们的组合。无机酸包括盐酸,硝酸,磷酸或硫酸。将磷处理的沸石与酸处理的无机氧化物粘合剂材料结合以形成沸石-粘合剂混合物。加水以形成可挤压的糊状物,该糊状物可以成形并加热到约4000℃或更高的温度以形成结合的磷改性沸石催化剂。对于芳族烷基化,在适合于芳族烷基化的反应条件下,使键合的磷改性沸石催化剂与芳族化合物和烷基化剂的芳族烷基化进料接触。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号