As for the P 2 O 5 -SiO 2 -Al 2 O 3 structure of the three-way flat panel display comprising a glass substrate, said ternary glass structure is resistant to high strain point temperature and the devitrification phenomenon, good chemical durability, and excellent insulating properties and thermal expansion It satisfies the condition of the silicon by a factor, and calculates a stable glass having a liquidus viscosity of possible forms in the traditional way. And it said glass composition comprises, based on the oxides of 33 to 75 weight% of P 2 O 5, 2 ~ 52 wt% of SiO 2 and 8 to 35% by weight of Al 2 O 3.; Three won structure, the liquidus and viscosity, display, aluminum
展开▼
机译:至于 P 2 O 5 -SiO 2 -Al 2 Sub> Sub> Sub> Sub> O 3的三元平面结构包含玻璃基板的面板显示器,所述三元玻璃结构耐高应变点温度和失透现象,良好的化学耐久性,以及优异的绝缘性能和热膨胀它满足硅的条件并计算出稳定的玻璃具有传统方式可能形式的液相线粘度。并且所述玻璃组合物基于33-75重量%的 P Sub> Sub> 2 O 5的氧化物,包含2〜52重量%的SiO 2 。 Sub>和8至35%的Al 2 Sub> O 3 Sub>。三韩元结构,液相线和粘度,显示,铝
展开▼