A Ni-added steel plate includes, by mass%, C: 0.04% to 0.10%, Si: 0.02% to 0.12%, Mn: 0.3% to 1.0%, Ni: more than 7.5% to 10.0%, Al: 0.01% to 0.08%, T-O: 0.0001 % to 0.0030%, P: limited to 0.0100% or less, S: limited to 0.0035% or less, N: limited to 0.0070% or less, and the balance consisting of Fe and unavoidable impurities, in which a Ni segregation ratio at an area of 1/4 of a plate thickness away from a plate surface in a thickness direction is 1.3 or less, a fraction of austenite after a deep cooling is 0.5% or more, an austenite unevenness index after the deep cooling is 3.0 or less, and an average equivalent circle diameter of the austenite after the deep cooling is 1 µm or less.
机译:添加了Ni的钢板,以质量%计,C:0.04〜0.10%,Si:0.02%〜0.12%,Mn:0.3%〜1.0%,Ni:大于7.5%〜10.0%,Al:0.01%至0.08%,TO:0.0001%至0.0030%,P:限制为0.0100%以下,S:限制为0.0035%以下,N:限制为0.0070%以下,其余部分由Fe和不可避免的杂质组成在板厚的1/4方向的板厚的厚度方向上的Ni偏析率为1.3以下,深冷后的奥氏体分率为0.5%以上,深度冷却为3.0以下,深度冷却后的奥氏体的平均等效圆直径为1μm以下。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号