The invention relates to a method of manufacturing a rare-earth doped alkaline-earth silicon nitride phosphor of a stoichiometric composition. Said method comprising the step of selecting one or more compounds each comprising at least one element of the group comprising the rare-earth elements (RE), the alkaline-earth elements (AE), silicon (Si) and nitrogen (N) and together comprising the necessary elements to form the rare-earth doped alkaline-earth silicon nitride phosphor (AE2Si5N8:RE). The method further comprises the step of bringing the compounds at an elevated temperature in reaction for forming the rare-earth doped alkaline-earth silicon nitride phosphor (AE2Si5N8:RE). In such a method normally a small amount of oxygen, whether intentionally or not-intentionally added, will be incorporated in the rare-earth doped alkaline-earth silicon nitride phosphor (AE2Si5N8:RE). According to the invention the creation of defects by formation of a non-stoichiometric oxygen containing phosphor is at least partly prevented by partly substituting for the ions (AE, Si, N) of the alkaline-earth silicon nitride phosphor (AE2Si5N8:RE) suitable further elements of the periodic system by which vacancies are created, filled or annihilated resulting in the formation of a modified alkaline-earth silicon nitride phosphor (AE2Si5N8:RE) having a stoichiometric composition. In this way a modified phosphor is obtained having excellent and stable optical properties. The invention further relates to a modified phosphor obtainable by the above-mentioned method and a radiation converting device comprising such a phosphor.
机译:本发明涉及一种化学计量组成的稀土掺杂碱土金属氮化硅磷光体的制造方法。所述方法包括以下步骤:选择一种或多种化合物,每种化合物包括稀土元素(RE),碱土元素(AE),硅(Si)和氮(N)以及一起的至少一种元素包含形成稀土掺杂的碱土金属氮化硅磷光体(AE2Si5N8:RE)的必要元素。该方法还包括使化合物在升高的温度下反应以形成稀土掺杂的碱土金属氮化硅磷光体(AE2Si5N8:RE)的步骤。在这种方法中,通常将有意或无意添加少量的氧气掺入稀土掺杂的碱土金属氮化硅荧光粉(AE2Si5N8:RE)。根据本发明,通过部分替代适合的碱土氮化硅磷光体(AE2Si5N8:RE)的离子(AE,Si,N),至少部分地防止了由于形成非化学计量的含氧磷光体而产生缺陷。周期系统的其他元素,通过这些元素可以产生,填充或消除空位,从而形成具有化学计量组成的改性碱土金属氮化硅磷光体(AE2Si5N8:RE)。以这种方式,获得了具有优异且稳定的光学性质的改性磷光体。本发明还涉及一种可通过上述方法获得的改性磷光体以及包括这种磷光体的辐射转换装置。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号