Instead of changing the polarizing film per se, by appropriately selecting the transparent protective film in consideration of the dimensional change of the polarizing film, the dimension of the polarizing film which can occur at the interface between the polarizing film and the transparent protective film (EN) Provided are an optical film laminate and the like capable of reducing stress caused by change. An optical film laminate including a polarizing film made of a polyvinyl alcohol resin having a dichroic substance oriented therein and having a thickness of 10 m or less and a transparent protective film made of a thermoplastic resin disposed on one side of the polarizing film with an adhesive layer interposed therebetween The transparent protective film has a thickness of 40 m or less and has a dimensional change rate in a direction perpendicular to the absorption axis of the polarizing film after leaving the test piece of 100 mm 100 mm in an environment of 85 C. for 48 hours Is 0.2% or more.