A method for leaching chalcopyrite concentrate by means of an aqueous solution containing sulfuric acid and an oxygen feed at atmospheric pressure and a temperature between 75 ° C and the boiling point of the solution, characterized by the fact that leaching is carried out in two-phase countercurrent leaching form in which the particle size of the concentrate to be fed to a first phase (1) of leaching is in the region of 80% below 60-100 μm, the concentrate is leached in the first leaching phase (1) with a leaching solution (5) leaving a second leaching phase with acid concentration in the region of 40-70 g / l (2) to form a solution (6) of copper sulfate having a regulated acid concentration in the region of 5-15 g / l; a residue (7) of the first phase (1) of leaching is fed to the second phase (2) of leaching, in which the residue is leached with a refining (8) whose acid concentration is regulated to be 20- 90 g / l
机译:一种在大气压力和75℃至溶液沸点之间的温度下,通过含有硫酸和氧气进料的水溶液浸出黄铜矿精矿的方法,其特征在于浸出是两相进行的。逆流浸出形式,其中将要进料到第一浸出阶段(1)的精矿的粒径在60-100μm以下80%的范围内,将精矿在第一浸出阶段(1)中用浸出溶液(5)离开第二个浸出阶段,酸浓度在40-70 g / l范围内(2)形成硫酸铜溶液(6),其硫酸浓度在5-15 g / l范围内l;将浸出的第一阶段(1)的残余物(7)送入浸出的第二阶段(2),在其中将残余物用精炼(8)浸出,其酸浓度调节为20- 90 g /升

著录项

  • 公开/公告号ES2617148T3

    专利类型

  • 公开/公告日2017-06-15

    原文格式PDF

  • 申请/专利权人 OUTOTEC (FINLAND) OY;

    申请/专利号ES20100791667T

  • 申请日2010-06-10

  • 分类号C22B3/08;C22B1;C22B15;

  • 国家 ES

  • 入库时间 2022-08-21 13:35:19

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号