Determination of the Optimum Conditions for Copper Leaching from Chalcopyrite Concentrate Ore Using Taguchi Method

机译:田口法确定黄铜矿精矿浸铜的最佳条件。

获取原文
获取原文并翻译 | 示例
           

摘要

The optimum conditions for the extraction of copper from chalcopyrite concentrate into SO2-saturated water were evaluated using the Taguchi optimization method. High level copper recovery was obtained in an environmentally friendly process that avoids sulfur dioxide emission into the atmosphere because SO2 forming in the roasting is used in the dissolution. Experimental parameters and their ranges were chosen as follows: reaction temperature, 293-333 K; solid-to-liquid ratio, 0.025-0.15 g/mL; roasting time, 30-90 min; roasting temperature, 773-973 K; stirring speed, 400-800 rpm; and reaction time, 10-60 min. The particle size and gas flow rate were 63 mm and 10 cm(3)/min, respectively. The optimum conditions of the dissolution process were determined to be reaction temperature of 318 K, a solid-to-liquid ratio of 0.025 gmL(-1), a roasting time of 75 min, a roasting temperature of 773 K, a stirring speed of 400 rpm, and a reaction time of 30 min. Under optimum conditions, dissolution yield of copper was 91%.
机译:使用Taguchi优化方法评估了从黄铜矿精矿中向SO2饱和水中提取铜的最佳条件。通过在环境友好的过程中获得高水平的铜回收率,避免了二氧​​化硫排放到大气中,因为在焙烧过程中使用了焙烧过程中形成的SO2。实验参数及其范围选择如下:反应温度293-333K;反应温度293-333K。固液比为0.025-0.15 g / mL;烘烤时间30-90分钟;焙烧温度773-973 K;搅拌速度400-800rpm;反应时间为10-60分钟。粒径和气体流速分别为63 mm和10 cm(3)/ min。确定溶解过程的最佳条件为:反应温度为318 K,固液比为0.025 gmL(-1),焙烧时间为75分钟,焙烧温度为773 K,搅拌速度为400 rpm,反应时间为30分钟。在最佳条件下,铜的溶出率为91%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号