Ba_(0.8)Sr_(0.2)TiO_3/YFeO_3 (BST/YIP) composites with giant dielectric constants and high saturation magnetizations were synthesized via the in-situ growth solid-state method. The BST/YIP composites were sintered at 1350℃, using Ba_(0.8)Sr_(0.2)TiO_3/YFeO_3 and Y_3Fe_5O_(12) as raw materials. The phase composition and surface morphology of the composites were investigated using XRD and SEM, respectively. The dielectric and magnetic properties of the composites were also studied. The results show that the BST/YIP composites have giant dielectric constants and high saturation magnetization. For the 40% BST/60% YIP composite, the dielectric constant and saturation magnetization are about 100,000 and 6.6, respectively. The giant dielectric constants of the BST/YIP composites are mainly attributed to the Maxwell-Wagner polarization.
机译:通过原位生长固态法合成了具有巨大介电常数和高饱和磁化强度的Ba_(0.8)Sr_(0.2)TiO_3 / YFeO_3(BST / YIP)复合材料。以Ba_(0.8)Sr_(0.2)TiO_3 / YFeO_3和Y_3Fe_5O_(12)为原料在1350℃烧结了BST / YIP复合材料。分别用XRD和SEM研究了复合材料的相组成和表面形态。还研究了复合材料的介电和磁性能。结果表明,BST / YIP复合材料具有巨大的介电常数和高饱和磁化强度。对于40%BST / 60%YIP复合材料,介电常数和饱和磁化强度分别约为100,000和6.6。 BST / YIP复合材料的巨大介电常数主要归因于Maxwell-Wagner极化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号