This article presents the effect of heat treating temperature on chemical composition of hydroxyapatite (HA) that was produced by burning bovine bone, and then heat treating the obtained bone ash at different temperatures in range of 600-1100 ℃ in air. Bone ash and the resulting white powder from heat treating were characterized by Fourier transformed infrared spectroscopy (FT-IR) and x-ray diffractometry (XRD). The FT-IR spectra confirmed that heat treating of bone ash at temperature of 800 ℃ removed the total of organic substances. x-ray diffraction analysis showed that the white powder was HA and HA was the only crystalline phase indicated in heat treating product. x-ray fluorescence analyses revealed that calcium and phosphorous were the main elements and magnesium and sodium were minor impurities of produced powder at 800 ℃. The results of the energy dispersive x-ray analysis showed that Ca/P ratio in produced HA varies in range of 1.46-2.01. The resulting material was found to be thermally stable up to 1100 ℃.
机译:本文介绍了热处理温度对燃烧牛骨产生的羟基磷灰石(HA)的化学成分的影响,然后在空气中600-1100℃的不同温度下对所得骨灰进行热处理。用傅里叶变换红外光谱(FT-IR)和X射线衍射仪(XRD)对骨灰和热处理产生的白色粉末进行表征。 FT-IR光谱证实,骨灰在800℃的温度下进行了热处理,除去了所有有机物。 X射线衍射分析表明,白色粉末是HA,并且HA是热处理产物中指示的唯一结晶相。 X射线荧光分析表明,在800℃时,钙和磷是主要成分,镁和钠是所生产粉末的微量杂质。能量色散X射线分析的结果表明,所产生的HA中的Ca / P比在1.46-2.01的范围内变化。发现所得材料在高达1100℃的温度下具有热稳定性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号