Films were prepared by casting alkaline solutions of gliadin, a major wheat storage protein fraction. Their compositions and mechanical and surface properties were analyzed. Five polyols of the ethylene glycol series and glycerol were compared as plasticizers. The plasticized film-forming solutions exhibited viscosities almost independent of shear rate. Glycerol-containing protein solutions had, however, a higher viscosity than others, after drying, concentrations of plasticizers in films were explained mainly, but not uniquely, by their volatility. At equal concentrations in films, glycerol and tetraethylene glycol were more efficient than the other plasticizers studied. A wide range of elongation (10-600%) was obtained when the plasticizer contents were varied, but the tensile strength (2-12 MPa) was always lower than that of usual synthetic polymer films. A negative relationship, independent of the plasticizing molecules used, was found between tensile strength and elongation at break of gliadin films. Surface hydrophobicity of films was high and no influence of plasticizers was observed. [References: 42]
机译:通过浇铸麦醇溶蛋白的碱性溶液来制备膜,麦醇溶蛋白是小麦的主要储藏蛋白部分。分析了它们的组成以及机械和表面性能。比较了五种乙二醇系列多元醇和甘油作为增塑剂。增塑的成膜溶液的粘度几乎与剪切速率无关。但是,含甘油的蛋白质溶液的粘度比其他溶液高,干燥后,主要但不是唯一地解释了它们中挥发性的增塑剂在薄膜中的浓度。在薄膜中浓度相同时,甘油和四甘醇比其他研究的增塑剂更有效。当增塑剂含量变化时,可以得到宽范围的伸长率(10-600%),但拉伸强度(2-12 MPa)始终低于通常的合成聚合物薄膜。发现在麦醇溶蛋白膜的拉伸强度和断裂伸长率之间存在负关系,而与所使用的增塑分子无关。膜的表面疏水性高,未观察到增塑剂的影响。 [参考:42]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号