首页> 外文期刊>Carbohydrate Polymers: Scientific and Technological Aspects of Industrially Important Polysaccharides >Stretching properties of xanthan, carob, modified guar and celluloses in cosmetic emulsions
【24h】

Stretching properties of xanthan, carob, modified guar and celluloses in cosmetic emulsions

机译:黄原胶,角豆树胶,改性瓜尔胶和纤维素在化妆品乳液中的拉伸性能

获取原文
获取原文并翻译 | 示例
           

摘要

The filament stretching properties of various polysaccharides (including xanthan, carob, hydroxypropyl guar, hydroxypropylmethyl and hydroxyethyl celluloses) were investigated and compared to synthetic polymers generally used as texturing agents in cosmetic emulsions. The stretchability was examined by sensory evaluation as "the amount of sample that strings rather than breaks when fingers are separated". Different behaviors were evidenced: the xanthan emulsion showed the highest stretchability, followed by the hydroxypropyl guar and hydroxyethyl cellulose emulsions while the synthetic polymers presented stretching properties to a much lesser extent. The instrumental characterization of the stretchability was conducted at a controlled speed and recorded with a camera using a texture analyzer. The maximum stretchable length at 40 mm/s was highly significantly correlated to the sensory Stringiness, thus allowing a good predictability of this attribute. Finally, this method was applied to aqueous solutions to better understand the role of the polymers in emulsion and to validate the measurement on a wider range of products.
机译:研究了各种多糖(包括黄原胶,角豆树胶,羟丙基瓜尔胶,羟丙基甲基和羟乙基纤维素)的长丝拉伸性能,并将其与化妆品乳液中通常用作变形剂的合成聚合物进行了比较。通过感官评价将拉伸性作为“手指分开时串而不是折断的样品量”。表现出不同的行为:黄原胶乳液显示出最高的可拉伸性,其次是羟丙基瓜尔胶和羟乙基纤维素乳液,而合成聚合物则表现出较小的拉伸性能。拉伸性的仪器表征以受控的速度进行,并使用质地分析仪用相机记录。 40 mm / s的最大可拉伸长度与感觉上的拉丝度高度相关,因此可以很好地预测此属性。最后,将此方法应用于水溶液,以更好地了解聚合物在乳液中的作用,并验证更广泛产品上的测量结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号