We synthesized core-shell microcapsule absorbents with crosslinked poly(acrylic acid) (PAA) as the core and poly(styrene-alt-maleic anhydride) (cPAA-PSMA) as the shell by the precipitation polymerization method for delayed absorption of excess water in cement mortar. To control the shell thickness, cPAA-PSMA capsules were synthesized with the core-to-shell monomer mass ratios of 1 : 0 (cPAA #1), 1 : 0.5 (cPAA-PSMA #2), 1 : 1 (cPAA-PSMA #3), and 1 : 1.5 (cPAA-PSMA #4). The viscosity of the cement paste with cPAA-PSMA #4 absorbent increased slowly until 90 minutes after absorbent addition, beyond which it increased rapidly. This suggests that mortars with cPAA-PSMA #4 absorbents can secure up to 90 minutes of working time. Incorporation of 1.0 wt% cPAA-PSMA #4 into cement mortar increased the compressive and flexural strengths by approximately 35% and 22%, respectively, compared to those of cement mortars without absorbents.
机译:我们通过沉淀聚合法合成了以交联聚丙烯酸(PAA)为核,聚苯乙烯-马来酸酐(cPAA-PSMA)为壳的核-壳型微胶囊吸收剂,以延迟吸收过量的水。水泥砂浆。为了控制壳的厚度,合成了cPAA-PSMA胶囊,其核壳比为1:0(cPAA#1),1:0.5(cPAA-PSMA#2),1:1(cPAA-PSMA #3)和1:1.5(cPAA-PSMA#4)。含cPAA-PSMA#4吸收剂的水泥浆的粘度缓慢增加,直到加入吸收剂后90分钟为止,然后迅速增加。这表明含有cPAA-PSMA#4吸收剂的砂浆可以确保长达90分钟的工作时间。与不含吸收剂的水泥砂浆相比,将1.0 wt%的cPAA-PSMA#4掺入水泥砂浆中的抗压强度和弯曲强度分别提高了约35%和22%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号