Study design This is a retrospective study comparing polyethylene wear between ceramic ball heads and metal ball heads in total hip arthroplasty. Background The ceramic-on-polyethylene bearing option has been introduced as an alternative to metal-on-polyethylene to minimize polyethylene wear debris and reduce subsequent osteolysis and aseptic loosening. However, the reported data were debatable. We designed this retrospective study to compare polyethylene wear between alumina ceramic ball heads and cobalt-chrome ball heads. Methods Bilateral simultaneous primary total hip arthroplasty was performed in 22 patients between January 2002 and December 2002, with one side using metal-on-polyethylene bearing surface and the other side using alumina ceramic-on-polyethylene bearing surface. After 10 years of follow-up, the wear rate of polyethylene liner on both sides was measured using the Dorr method and compared. Results The annual wear rate of the polyethylene liner was 0.133 mm with a standard deviation of 0.045 in the metal-on-polyethylene group and 0.056 mm with a standard deviation of 0.032 in the ceramic-on-polyethylene group. The wear rate per year was significantly lower in the ceramic-on-polyethylene group ( p Conclusions Although the implication is still controversial, our study showed that the use of ceramic head lowered the liner wear rate. Clinical relevance Ceramic is harder and more resistant to scratching than cobalt-chrome. By increasing polyethylene liner survivorship and decreasing potential osteolytic response and aseptic loosening, ceramic head is a better alternative than cobalt-chrome head.
机译:研究设计这是一项回顾性研究,比较了全髋关节置换术中陶瓷球头和金属球头之间的聚乙烯磨损。背景技术已经引入了聚乙烯上的陶瓷轴承选件,以替代聚乙烯上的金属,以最大程度地减少聚乙烯磨损碎片并减少随后的骨溶解和无菌性松动。但是,报告的数据值得商bat。我们设计了这项回顾性研究,以比较氧化铝陶瓷球头和钴铬球头之间的聚乙烯磨损。方法2002年1月至2002年12月,对22例患者同时进行双侧原发性全髋关节置换术,一侧使用金属-聚乙烯基表面,另一侧使用氧化铝陶瓷-聚乙烯基表面。经过10年的随访,使用Dorr方法测量了聚乙烯衬里两侧的磨损率并进行了比较。结果聚乙烯衬里的年磨损率是0.133 mm,金属在聚乙烯上的标准偏差为0.045,0.056 mm,在陶瓷上的聚乙烯的标准偏差为0.032。聚乙烯基陶瓷涂层组的年磨损率显着降低(p结论尽管这一含义仍存在争议,但我们的研究表明,使用陶瓷头降低了衬管的磨损率。通过增加聚乙烯衬垫的存活率并减少潜在的溶骨反应和无菌性松动,陶瓷头比钴铬头更好。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号