首页> 外文期刊>Applied Surface Science >Laser assisted fabrication of micro-lens array and characterization of their beam shaping property
【24h】

Laser assisted fabrication of micro-lens array and characterization of their beam shaping property

机译:激光辅助制造微透镜阵列及其梁成型性的表征

获取原文
获取原文并翻译 | 示例

摘要

This paper demonstrates the formation of high-fill-factor plano-convex cylindrical and dome-type micro-lens arrays on fused silica glass surface using CO2 laser assisted reshaping technique. Cylindrical micro-lens array is fabricated by polishing the femtosecond laser engraved linear micro-gratings by a CO2 laser beam. Initially, a femtosecond laser beam has been irradiated on the surface of the fused silica glass samples to fabricate periodic micro-gratings on the glass surface. Afterwards, these micro-gratings encoded glass samples are polished several times by a CO2 laser beam. As a result, plano-convex cylindrical micro-lens arrays with the lens period varying from 20 mu m to 50 mu m are developed on the glass surface. Similarly, dome-type micro-lens array is achieved by femtosecond laser assisted fabrication of periodic micro-pillars followed by several times CO2 laser polishing. We report the formation of a large variety of dome-shape micro-lens array with lens size varying from 20 mu m x 20 mu m to 50 mu m x 50 mu m. The fabricated micro-lenses show great consistency in size and shape throughout the sample area. We also investigate the intensity distribution of light passed through the micro-lens engraved glass samples. Using the dome-type micro-lens array engraved glass samples, a Gaussian laser beam has been converted to a flat-top laser beam for selective patterning of a thin indium-tin-oxide coating from fused silica glass surface.
机译:本文展示了使用CO2激光辅助重塑技术在熔融石英玻璃表面上形成高填充因子Plano-凸圆柱和圆顶型微透镜阵列。通过CO2激光束抛光飞秒激光雕刻的线性微光栅来制造圆柱形微透镜阵列。最初,在熔融石英玻璃样品的表面上照射了飞秒激光束,以制造在玻璃表面上的周期性微光栅。然后,通过CO 2激光束抛光这些微光栅编码玻璃样品。结果,在玻璃表面上显影的具有从20μm至50μm的镜头周期变化的透镜周期的平面凸圆柱微透镜阵列。类似地,圆顶型微透镜阵列通过飞秒激光辅助制造的周期性微柱,其次是多次CO2激光抛光。我们报告了各种各样的圆顶微透镜阵列的形成,镜头尺寸不同于20亩×20μm至50 mu m x 50 mu m。制造的微透镜在整个样本区域的尺寸和形状上显示出很大的稠度。我们还研究了通过微透镜雕刻玻璃样品的光的强度分布。使用圆顶型微透镜阵列雕刻玻璃样品,高斯激光束已被转换为平顶激光束,以便从熔融石英玻璃表面选择薄铟锡氧化物涂层的选择性图案化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号