Hydrophilization of Poly(Caprolactone) Copolymers through Introduction of Oligo(Ethylene Glycol) Moieties

机译:通过引入低聚(乙二醇)部分使聚己内酯共聚物亲水化

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

In this study, a new family of poly(ε-caprolactone) (PCL) copolymers that bear oligo(ethylene glycol) (OEG) moieties is described. The synthesis of three different oligo(ethylene glycol) functionalized epoxide monomers derived from 2-methyl-4-pentenoic acid, and their copolymerization with ε-caprolactone (CL) to poly(CL-co-OEG-MPO) copolymers is presented. The statistical copolymerization initiated with SnOct2/BnOH yielded the copolymers with varying OEG content and composition. The linear relationship between feed ratio and incorporation of the OEG co-monomer enables control over backbone functional group density. The introduction of OEG moieties influenced both the thermal and the hydrophilic characteristics of the copolymers. Both increasing OEG length and backbone content resulted in a decrease in static water contact angle. The introduction of OEG side chains in the PCL copolymers had no adverse influence on MC-3TE3-E1 cell interaction. However, changes to cell form factor (Φ) were observed. While unmodified PCL promoted elongated (anisotropic) morphologies (Φ = 0.094), PCL copolymer with tri-ethylene glycol side chains at or above seven percent backbone incorporation induced more isotropic cell morphologies (Φ = 0.184) similar to those observed on glass controls (Φ = 0.151).
机译:在这项研究中,描述了一个新的带有低聚乙二醇(OEG)部分的聚(ε-己内酯)(PCL)共聚物。介绍了三种不同的由2-甲基-4-戊烯酸衍生的低聚乙二醇官能化的环氧单体的合成,以及它们与ε-己内酯(CL)共聚成聚(CL-co-OEG-MPO)共聚物的过程。用SnOct2 / BnOH引发的统计共聚反应产生了具有不同OEG含量和组成的共聚物。进料比与OEG共聚单体的掺入之间的线性关系使得能够控制主链官能团密度。 OEG部分的引入影响了共聚物的热和亲水特性。 OEG长度的增加和主链含量的增加都导致静水接触角的减小。在PCL共聚物中引入OEG侧链对MC-3TE3-E1细胞相互作用没有不利影响。但是,观察到细胞形状因子(Φ)的变化。未改性的PCL促进了伸长的(各向异性)形态(Φ= 0.094),而具有三乙二醇侧链的骨架主链掺入率为7%或更高的PCL共聚物则诱导了更多各向同性的细胞形态(Φ= 0.184),类似于玻璃对照(Φ) = 0.151)。