首页> 美国卫生研究院文献>Nanoscale Research Letters >Effects of crystallization and dopant concentration on the emission behavior of TiO2:Eu nanophosphors
【2h】

Effects of crystallization and dopant concentration on the emission behavior of TiO2:Eu nanophosphors

机译:结晶和掺杂剂浓度对TiO2:Eu纳米磷光体发射行为的影响

代理获取
本网站仅为用户提供外文OA文献查询和代理获取服务,本网站没有原文。下单后我们将采用程序或人工为您竭诚获取高质量的原文,但由于OA文献来源多样且变更频繁,仍可能出现获取不到、文献不完整或与标题不符等情况,如果获取不到我们将提供退款服务。请知悉。

摘要

Uniform, spherical-shaped TiO2:Eu nanoparticles with different doping concentrations have been synthesized through controlled hydrolysis of titanium tetrabutoxide under appropriate pH and temperature in the presence of EuCl3·6H2O. Through air annealing at 500°C for 2 h, the amorphous, as-grown nanoparticles could be converted to a pure anatase phase. The morphology, structural, and optical properties of the annealed nanostructures were studied using X-ray diffraction, scanning electron microscopy, energy-dispersive X-ray spectroscopy [EDS], and UV-Visible diffuse reflectance spectroscopy techniques. Optoelectronic behaviors of the nanostructures were studied using micro-Raman and photoluminescence [PL] spectroscopies at room temperature. EDS results confirmed a systematic increase of Eu content in the as-prepared samples with the increase of nominal europium content in the reaction solution. With the increasing dopant concentration, crystallinity and crystallite size of the titania particles decreased gradually. Incorporation of europium in the titania particles induced a structural deformation and a blueshift of their absorption edge. While the room-temperature PL emission of the as-grown samples is dominated by the 5D0 - 7Fj transition of Eu+3 ions, the emission intensity reduced drastically after thermal annealing due to outwards segregation of dopant ions.
机译:通过在EuCl3·6H2O的存在下,在适当的pH和温度下控制四丁氧基钛的水解,合成了具有不同掺杂浓度的均匀球形TiO2:Eu纳米颗粒。通过在500°C下空气退火2小时,非晶态的,生长态的纳米颗粒可以转化为纯锐钛矿相。使用X射线衍射,扫描电子显微镜,能量色散X射线光谱[EDS]和紫外可见漫反射光谱技术研究了退火纳米结构的形貌,结构和光学性质。在室温下使用微拉曼光谱和光致发光[PL]光谱学研究了纳米结构的光电行为。 EDS结果证实,随着反应溶液中标称content含量的增加,制得的样品中Eu含量有系统的增加。随着掺杂剂浓度的增加,二氧化钛颗粒的结晶度和晶粒尺寸逐渐减小。在二氧化钛颗粒中掺入induced会引起结构变形和吸收边缘的蓝移。虽然生长中的样品的室温PL发射主要由Eu +3 离子的 5 D0- 7 Fj跃迁控制,由于掺杂离子的向外偏析,在热退火之后,发射强度急剧降低。