This paper reports on preparation and characterization of Potassium Dihydrogen Phosphate (KDP) crystals doped with Potassium Dichromate (PD). The crystals were grown at room temperature by solution evaporation technique. The grown crystals were polished, sliced, and analyzed using UV-Spectrophotometer, which showed high concentration of PD impurities in KDP crystals at 200-280 nanometer. These concentrations were then verified using ICP measurements to determine specific amount in ppm of chromium ions in KDP crystals. In additional to that, the UV-transmittance data of these crystals were then converted to absorbance per thickness, and used to calculate absorption coefficients, extinction coefficients, and refractive index as a function of wavelength. The results showed that the presence of PD impurities in the crystal matrix of KDP has played a key reformative role in the UV sensing of Potassium Diphosphate crystals.
机译:本文报道了磷酸二甲酸钾(Pd)掺杂磷酸钾(KDP)晶体的制备和表征。通过溶液蒸发技术在室温下生长晶体。使用UV-分光光度计抛光,切割和分析生长的晶体,其在200-280纳米的KDP晶体中显示出高浓度的PD杂质。然后使用ICP测量验证这些浓度以确定KDP晶体中PPM中PPM的特定量。然后,随着该晶体的UV透射率数据,然后将其厚度的吸光度转化为吸光度,并且用于计算吸收系数,消光系数和折射率作为波长的函数。结果表明,KDP晶体基质中Pd杂质的存在在二磷酸二磷酸钾的紫外线感测中发挥了关键重整作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号