Influence of Type of Secondary Raw Material on Consistency of Fresh Mixture for AAC Production

机译:二次原料型对AAC生产新混合物稠度的影响

获取原文

摘要

Autoclaved aerated concrete (AAC) is, mainly in Europe, widely used construction material. It has an optimal combination of bulk density, strength and thermal conductivity coefficient for load-bearing and non-load-bearing structures of civil facilities. The production technology is based on a mixture of ground silica sand, lime, cement, gypsum, aluminium powder and additives. The grinding of sand is most often carried out in a wet way, and the sand sludge is consequently used in production technology. The aim of the experiment was verification of the effect of partial replacement of sand with the alternative raw materials in sand sludge on the rheology of the mixture. This parameter determinates how the modified mixtures affect the sludge pumpability. As a reference the consistency of the sand sludge of the normal production density of 1.65 g/cm~3 was compared to the sand sludges of different density (1.60, 1.70 and 1.75 g/cm~3) and with a fresh aerated concrete (FAC) mixture of 1.60 g/cm~3. Then the sludges were modified by 30 % of alternative raw materials (recycled glass, coal slag, FBC ash, FBC bottom ash) as the partial weight replacement for sand. This partial replacement resulted in water/solids ratio adjustment which recommended value is 0.47 for recycled glass and coal slag, 0.59 for fluidized bed combustion (FBC) bottom ash and for FBC fly ash it is 0.70.
机译:高压灭菌的混凝土(AAC)主要在欧洲,广泛使用的建筑材料。它具有堆积密度,强度和导热系数的最佳组合,用于承载的承载和防护装置的非承重结构。生产技术基于地面二氧化硅砂,石灰,水泥,石膏,铝粉和添加剂的混合物。沙子的研磨最常以湿润方式进行,因此在生产技术中使用砂污泥。实验的目的是验证砂砂中砂污染的替代原料的抗体效果验证了混合物流变学中的替代原料。该参数确定改性混合物如何影响污泥泵送性。作为参考,将正常生产密度为1.65g / cm〜3的砂污泥的一致性与不同密度(1.60,1.70和1.75g / cm〜3)的砂污泥进行比较,并用新鲜的气化混凝土(FAC )1.60g / cm〜3的混合物。然后将污泥的30%改性替代原料(再生玻璃,煤渣,FBC灰,FBC底灰)作为砂的部分重量替代。这种部分替代导致水/固体比调节,用于再生玻璃和煤渣的推荐值为0.47,0.59用于流化床燃烧(FBC)底灰和FBC粉煤灰为0.70。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号