Acoustic emission and electrical properties of quasi-brittle materials under compression

机译:压缩下准脆性材料的声发射和电性能

获取原文

摘要

Acoustic emission (AE), electromagnetic emission (EME) and electrical properties measurements have been performed during laboratory compression tests on Green Luserna Granite dry rock loaded with increasing pressure up to their failure. Using a servo-controlled testing machine (MTS) each compression test was carried out at constant displacement rate and under ordinary room conditions. AE signals were detected by applying to the sample surface a piezoelectric (PZT) transducer, sensitive in the frequency range from 50 to 500 kHz. EME signals were detected using a loop antenna (80.0 dB gain at 500 kHz). The time-dependent outputs of the PZT transducer and the electromagnetic tester were connected to a DL708 Yokogawa oscilloscope (10 MSa s~(-1)) in order to acquire simultaneously AE and EME signals associated with the same fracture event. Electrical properties, in terms of relative electrical resistance variation, were monitored by using copper electrodes coupled to specimens by conductive silver paint, and connected to a multimeter (Agilent model 34411A). The recorded AE, EME and electrical properties variation were related to the load vs. time diagram of the tested specimens. The experiments conducted in this research confirm that AE and EME are failure precursors in quasi-brittle materials, moreover EME signals and electrical property variations are related to sharp drops in stress vs. time diagram.
机译:在载入的绿色Luserna花岗岩干燥岩石上的实验室压缩测试期间,已经进行了声发射(AE),电磁发射(EME)和电学特性测量。使用伺服控制的试验机(MTS),每个压缩测试以恒定的位移率和普通空间条件下进行。通过向样品表面施加压电(PZT)换能器来检测AE信号,在50至500kHz的频率范围内敏感。使用环形天线检测EME信号(800 kHz的80.0 dB增益)。 PZT换能器和电磁测试器的时间依赖性输出连接到DL708横川示波器(10MSA S〜(-1)),以便同时获取与相同骨折事件相关的AE和EME信号。在相对电阻变化方面,通过使用导电银涂料耦合到样本的铜电极来监测电特性,并连接到万用表(Agilent Model 34411a)。记录的AE,EME和电性能变化与测试样本的负载与时间图有关。本研究中进行的实验证实,AE和EME是准脆性材料中的失效前体,此外,EME信号和电性能变化与应力与时间图中的尖锐下降有关。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号