首页> 外国专利> MANUFACTURING METHOD FOR MOLDED ARTICLE USING FIBER REINFORCERD PLASTIC WASTE COMPRISING THERMOSETTING PLASTICS AND MOLDED ARTICLE USING THE SAME

MANUFACTURING METHOD FOR MOLDED ARTICLE USING FIBER REINFORCERD PLASTIC WASTE COMPRISING THERMOSETTING PLASTICS AND MOLDED ARTICLE USING THE SAME

机译:模塑制品用纤维增强塑料废物制造方法,包括使用热固性塑料和模塑制品

摘要

The present invention relates to a method for manufacturing a molded article using waste fiber-reinforced plastic containing a thermosetting resin and to a molded article produced thereby. The method for manufacturing a molded article using the waste fiber-reinforced plastic includes: pulverizing the waste fiber-reinforced plastic to a size of 1 μm to 80 μm to prepare a pulverized product; And pressurizing the pulverized product at 150 ~ 250 ℃; is a molded body manufacturing method using a waste fiber-reinforced plastic comprising; the waste fiber-reinforced plastic is a thermosetting matrix resin 35 ~ 90% by weight and impregnated in the thermosetting matrix resin It contains 10 to 65% by weight of a fiber filler, the molded body is made of only the waste fiber-reinforced plastic, and the manufactured molded body has a compressive strength of 30 to 60 MPa measured based on ASTM D 695 standard.
机译:本发明涉及一种使用含有热固性树脂的废纤维增强塑料和由此制备的模塑制品制造模塑制品的方法。 使用废纤维增强塑料制造模塑制品的方法包括:将废纤维增强塑料粉碎至1μm至80μm的尺寸以制备粉碎的产品; 并在150〜250℃加压粉碎产品; 是使用废纤维增强塑料的模塑体制造方法; 废纤维增强塑料是热固性基质树脂35〜90重量%,浸渍在热固性基质树脂中,含有10至65重量%的纤维填料,模制体仅由废纤维增强塑料制成 并且,制造的模塑主体基于ASTM D 695标准测量的抗压强度为30至60MPa。

著录项

  • 公开/公告号KR102291931B1

    专利类型

  • 公开/公告日2021-08-23

    原文格式PDF

  • 申请/专利权人 주식회사 엔이티;

    申请/专利号KR20200012728

  • 发明设计人 김길수;구병회;

    申请日2020-02-03

  • 分类号B29C70/02;B29B13/10;B29B9/14;B29K105/26;

  • 国家 KR

  • 入库时间 2024-06-14 22:23:27

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号