首页> 外国专利> Manufacturing method of optical casting having holographic optical element

Manufacturing method of optical casting having holographic optical element

机译:具有全息光学元件的光学铸件的制造方法

摘要

The present invention relates to a method for producing an optical casting comprising at least one volume holographic optical element by a casting process, the method comprising the following steps: a flat, spherical, non-spherical or free-form first surface Providing a casting mold (30) comprising a first mold part (10) having a second mold part (20) having a flat, spherical, non-spherical or free-form second surface. Providing a first mold part (10) connectable to the second mold part (20) to form a casting mold (30); providing at least one holographic optical element (91) Placing the at least one holographic optical element (91) relative to the first mold part (10) and / or the second mold part (20). Aligning the first mold part and the second mold part to form the casting mold (30); introducing the casting material into one or more casting processes, The casting material having a maximum viscosity of 100,000 mPas at 25 ° C .; curing the casting material; removing the cured casting material comprising at least one holographic optical element (91) from the casting mold (30) A casting material extending at least partially around at least one holographic optical element (91). [Selection] Figure 2
机译:本发明涉及一种用于制造包括通过铸造工艺的至少一个体积全息光学元件的光学铸件的方法,该方法包括以下步骤:扁平,球形,非球形或自由形式的第一表面,提供铸造模具(30)包括第一模具部分(10),第一模具部分(10)具有具有平坦的,球形,非球形或自由形状的第二表面的第二模具部分(20)。提供连接到第二模具部分(20)的第一模具部分(10),以形成铸造模具(30);提供至少一个全息光学元件(91)将所述至少一个全息光学元件(91)放置在第一模具部分(10)和/或第二模具部分(20)上。将第一模具部分和第二模具部件对准以形成铸模(30);将铸造材料引入一个或多个铸造过程中,铸造材料在25℃下具有100,000mPas的最大粘度。;固化铸造材料;去除包括从铸模(30)的至少一个全息光学元件(91)的固化铸造材料,铸造材料至少部分地围绕至少一个全息光学元件(91)延伸。 [选择]图2

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号