Provided is a method for producing a structure catalyst for generating a high-concentration hydrogen gas by a water-gas shift reaction from a gas containing hydrogen and carbon monoxide. The method for producing the structure catalyst includes an anoxidation step (S1) in which the surface of the aluminum substrate is annotated to form an alumina carrier, and a first immersion step in which the alumina carrier is immersed in an aqueous solution containing a catalyst component. (S4), the first firing step (S5) in which the alumina carrier on which a partial amount of the catalyst component is supported in the first immersion step is fired in a temperature range of 120 to 500 ° C. in an oxidizing atmosphere, and the above. A second dipping step (S6) in which the alumina carrier that has undergone the first firing step is immersed in an aqueous solution containing the catalyst component, and the alumina in which the final amount of the catalyst component is supported in the second dipping step. The second firing step (S7) of firing the carrier in a temperature range of 120 to 500 ° C. in an oxidizing atmosphere is performed.
机译:提供了一种制备结构催化剂的方法,其通过从含有氢气和一氧化碳的气体的水 - 气体移反应产生高浓度氢气。制备结构催化剂的方法包括氧化氧化步骤(S1),其中铝基板的表面被注释以形成氧化铝载体,以及第一浸渍步骤,其中氧化铝载体浸入含有催化剂组分的水溶液中。 (S4),第一烧制步骤(S5),其中在第一浸渍步骤中催化催化剂组分的部分量的氧化铝载体在氧化气氛中在120-500℃的温度范围内烧制,和上面的。第二浸渍步骤(S6),其中经过第一烧制步骤的氧化铝载体浸入含有催化剂组分的水溶液中,以及其中催化剂组分的最终量的氧化铝在第二次浸渍步骤中负载。进行在氧化气氛中在120至500℃的温度范围内烧制载体的第二烧制步骤(S7)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号