557,109. Reproducing drawings. KODAK, Ltd. (Eastman Kodak Co., Wynd, C. L. A., and Lane, G T.). April 29, 1942, No. 5786. [Classes 98 (i) and 98 (ii)] [Also in Group XL] In the photographic reproduction of engineering drawings and like patterns an original drawing is made in fluorescent material which is on an opaque support say of aluminium or plywood permeable to X-rays. On a second similar support are superposed (i) a layer of fluorescent material, (ii) a light filter or screening material, and (iii) a light sensitive emulsion. The original drawing is now reproduced on the emulsion and during the fixing process or by other means the light filter or screen-which was opaque to light -is made transparent. By this means mirror images of the original drawing are obtained, which can be used to obtain symmetrical templates for example templates of the right and left hand doors of an automobile. The luminescent layer may be calcium tungstate in a cellulose ester solution which is water resistant, or barium fluorochloride in a binder as described in Specification 557,102 may be used. The screening layer may be manganese dioxide or a non- wandering dye in gelatine, a cellulose ester partially hydrolysed until water permeable, or a resin. The sensitive layer may be applied by the methods described in Specifications 553,341, 554,292 and 549,371. The fluorescent material may be activated by U.V. or cathode rays or, if the radiation will not pass through the support, phosphorescent means may be used. Specification 548,795 also is referred to.
展开▼
机译:557,109。复制图纸。柯达有限公司(Eastman Kodak Co.,Wynd,C. L. A.,and Lane,G T.)。 1942年4月29日,编号5786。[98(i)和98(ii)类] [也在XL组中]在工程图和类似图案的照相复制中,原始图是用不透明的荧光材料制成的支持说铝或胶合板可以透过X射线。在第二个类似的支撑物上叠加(i)一层荧光材料,(ii)滤光器或屏蔽材料以及(iii)光敏乳剂。现在将原始图形复制到乳剂上,并在定影过程中或通过其他方式使对光不透明的滤光器或屏幕透明。通过这种方式,获得了原始图的镜像,该镜像可用于获得对称模板,例如汽车左右门的模板。发光层可以是耐水的纤维素酯溶液中的钨酸钙,或者可以使用规范557,102中所述的粘合剂中的氟化氯钡。屏蔽层可以是二氧化锰或明胶中的无漂移染料,部分水解直至透水的纤维素酯或树脂。可以通过规范553,341、554,292和549,371中描述的方法来施加敏感层。荧光材料可以通过紫外线激活。或阴极射线,或者,如果辐射不会通过载体,则可以使用磷光装置。还参考了规格548,795。
展开▼