首页> 外国专利> METHOD OF PRODUCING BULKY TEXTURED HYBRID YARN AND YARN PRODUCED THEREBY

METHOD OF PRODUCING BULKY TEXTURED HYBRID YARN AND YARN PRODUCED THEREBY

机译:生产大块状混纺纱的方法及由此产生的纱

摘要

1513927 Bulking yarn by fluid texturing and heat shrinking VYZKUMNY USTAV PLETARSKY 29 Aug 1975 [6 Sept 1974] 35666/75 Headings D1F and DIW A hybrid textured and bulked yarn is obtained by passing threads 3, 5 of different shrinkability through a turbulent fluid texturing nozzle 10 to produce crimps and loops and intermingle the threads, and heat shrinking at least the more shrinkable threads to produce in them a specific shrinking stress of at least 0.1 p/dtex so as to enlarge and set the crimps and loops by passing the textured yarn 12 through heater 13. Generally the threads 3, 5 are each multicontinuous filament yarns but in example 3 the less shrinkable threads are supplied as a roving of staple polyester fibres and in example 4 the more shrinkable threads are staple copolyester fibres. The specified more shrinkable thread is an ethylene terephthalate/isophthalate copolymer of 40% shrinkability. The threads of lower shrinkability are of polyester, nylon, rayon, acrylics or polypropylene. In example 1 polyester filaments of 10% shrinkability are fed to nozzle 10 with 20% overfeed and copolyester filaments of 40% shrinkability are fed with 10% overfeed. The textured yarn is shrunk by heating to 150‹C. In example 2 filaments of different shrinkability are obtained from the same polymer by drawing one freshly extruded filament over one heater whilst another filament is drawn over two heaters. The bending moment may be reduced at intervals along the filaments by flattening or otherwise changing the filament crosssection, so as to make the length and frequency of the loops more controllable.
机译:1513927通过流体变形和热收缩来膨松纱线VYZKUMNY USTAV PLETARSKY 1975年8月29日[1974年9月6日] 35666/75机头D1F和DIW通过将具有不同收缩率的线3、5通过湍流的流体变形喷嘴来获得混合膨松纱10产生卷曲和环并混入线,并热收缩至少收缩率更高的线以在它们中产生至少0.1 p / dtex的比收缩应力,以便通过使变形纱通过来增大和设置卷曲和环线12、12通常通过加热器13。通常,线3、5是多连续长丝纱线,但是在实施例3中,收缩性较低的线作为短聚酯纤维的粗纱供应,而在实施例4中,收缩性较大的线是短共聚酯纤维。指定的更具收缩性的线是收缩率40%的对苯二甲酸乙二酯/间苯二甲酸酯共聚物。收缩率较低的线是聚酯,尼龙,人造丝,丙烯酸或聚丙烯。在实施例1中,将具有10%可收缩性的聚酯长丝以20%的过量进料供给到喷嘴10,并且将具有40%可收缩性的共聚酯长丝以10%的过量进料供给。通过加热至150℃将变形纱收缩。在实施例2中,通过在一个加热器上拉伸一根新挤出的长丝,而在两个加热器上拉伸另一根长丝,从相同的聚合物获得具有不同收缩率的长丝。弯曲力矩可以通过变平或以其他方式改变细丝横截面而沿着细丝以一定间隔减小,从而使环的长度和频率更可控。

著录项

  • 公开/公告号GB1513927A

    专利类型

  • 公开/公告日1978-06-14

    原文格式PDF

  • 申请/专利权人 VYZKUMNY USTAV PLETARSKY;

    申请/专利号GB19750035666

  • 发明设计人

    申请日1975-08-29

  • 分类号D02G1/16;D02G1/18;D02G1/20;

  • 国家 GB

  • 入库时间 2022-08-22 21:37:39