首页> 外国专利> ENDHAT FOR MAGNETRON

ENDHAT FOR MAGNETRON

机译:这场战争是磁控管

摘要

PURPOSE:To have the brazing work carried out effeciently in the process of assembling a magnetron by sticking the brazing material beforehand to the place to be fused and also to reduce the production cost well to be applied to an electronic range etc. by utilizing low-priced ruthenium and molybdenum as a brazing material. CONSTITUTION:Brazing of an end hat proper with a lead rod 4 can be carried out, by a method wherein another brazing material 5' in addition to a ring- shaped brazing material 5 is kept intact on the enhat 5 then heated and the space between the lead rod 4 and a fitting inlet 1d installed on a cylindrical part 1c is impregnated with molten brazing material, hence D1 is 8.5mm., D2 is 4.07mm., d is 1.55mm., H is 2.0mm., t is 0.5mm., and t' is 1.5mm.. Also, with respect to the dimension of the ring-shaped brazing material, the outside diameter is 8mm., the inside diameter is 4.3mm. and the thickness is 0.3mm., and it is stuck to the endhat proper 1a made of molybdenum by means of vinyl-system adhesive.
机译:目的:通过预先将钎焊材料粘贴到要熔化的地方,在组装磁控管的过程中有效地进行钎焊工作,并通过降低成本来降低生产成本,从而可很好地应用于电子炉等。标价的钌和钼作为钎焊材料。组成:可以用一种方法用引线杆4钎焊端帽,方法是:除环形钎焊材料5外,将另一种钎焊材料5'完整地保持在密封帽5上,然后加热,引线4和安装在圆筒形部件1c上的装配入口1d被熔融的钎料浸渍,因此D1为8.5mm,D2为4.07mm,d为1.55mm,H为2.0mm,t为0.5另外,关于环状钎焊材料的尺寸,外径为8mm,内径为4.3mm。厚度为0.3mm,并通过乙烯基系粘合剂粘结到由钼制成的端帽本体1a上。

著录项

  • 公开/公告号JPS6035781B2

    专利类型

  • 公开/公告日1985-08-16

    原文格式PDF

  • 申请/专利权人 TOHO KINZOKU KK;

    申请/专利号JP19810152701

  • 发明设计人 FURUYAMA RYUNOSUKE;

    申请日1981-09-25

  • 分类号H01J23/04;H01J23/05;

  • 国家 JP