首页> 外国专利> FOERFARANDE FOER AVSKILJNING AV TELLURIUM AV KOPPARELEKTRORAFFINERINGSSLAM.

FOERFARANDE FOER AVSKILJNING AV TELLURIUM AV KOPPARELEKTRORAFFINERINGSSLAM.

机译:分离铜电渣油中的碲的方法。

摘要

A method of increasing the extraction of tellurium from copper electrorefining slime comprises leaching the slime with dilute sulphuric acid in a reactor under a partial oxygen pressure of up to 150 psi and at an elevated temperature between about 100 and 200 DEG C until copper, nickel and substantially all of the tellurium is dissolved, thereby forming a leach slurry, and contacting the slurry with an appropriate reducing agent immediately after the leaching operation has been halted and the leaching reactor brough back to atmospheric pressure to reprecipitate any excessive quantities of silver and selenium solubilized during the leaching operation.
机译:一种增加从铜电精炼煤泥中提取碲的方法,该方法包括在反应器中在最高150 psi的分氧气压和约100至200℃的高温下,用稀硫酸浸出煤泥,直至铜,镍和镍。基本上所有的碲都溶解了,从而形成了浸出浆液,并且在浸出操作停止并且浸出反应器鼓吹回到大气压以立即沉淀出任何过量的银和硒后,立即使浆液与适当的还原剂接触。在浸出操作中。

著录项

  • 公开/公告号FI923649A0

    专利类型

  • 公开/公告日1992-08-14

    原文格式PDF

  • 申请/专利权人 NORANDA INC.;

    申请/专利号FI19920003649

  • 发明设计人 CLAESSENS PIERRE L.;WHITE CARL W.;

    申请日1992-08-14

  • 分类号C25C;

  • 国家 FI

  • 入库时间 2022-08-22 05:35:40