Polymer materials with high fire resistance (I), contain prim. or sec. thermoplastics and fillers for parts which are used at high temp., e.g. in metallurgical processes. (I) contain 60-97 wt.% high- or low-pressure polyethylene, polypropylene or polystyrene, or a mixt. contg. 0.1-75 wt.% of each component (II), and 3-40 wt.% dried water-glass (III) and/or 1-30 wt.% dried lignin and/or 5-30 wt.% temp.-activated zeolite. (I) are produced, e.g. in the form of tubes, by drying (III) at 100-210 deg.C, grinding to 0.3-1 mm particle size, mixing with polymer (II) and extruding at 90-200 deg C (i.e. at least 10-15 deg C below the drying temp. for III). USE/ADVANTAGE - (I) are useful, e.g. for the prodn. of protecting tubes for probes for the periodic measurement of temp. in steel prodn.. Fire resistant materials can be simply produced and do not required special conditions for storage. (0/0)
机译:具有高耐火性(I)的聚合物材料包含底漆。或秒用于高温的零件的热塑性塑料和填料,例如在冶金过程中。 (I)包含60-97重量%的高压或低压聚乙烯,聚丙烯或聚苯乙烯或混合物。续每种组分(II)为0.1-75 wt。%,干燥的水玻璃(III)为3-40 wt。%,和/或干燥的木质素为1-30 wt。%,和/或温度为5-30 wt。%。活性沸石。 (I)被生产,例如以管形式,通过在100-210℃下干燥(III),研磨至0.3-1mm的粒度,与聚合物(II)混合并在90-200℃下挤出(即至少10-15℃) C低于III的干燥温度。使用/优势-(I)是有用的,例如为产品用于定期测量温度的探头保护管耐火材料可以简单地生产,不需要特殊的存储条件。 (0/0)

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号