METHOD OF MANUFACTURING BRIQUETS FOR DIRECTLY ALLOYING STEEL WITH MANGANESE

机译:用锰直接合金化钢的加工方法。

摘要

FIELD: ferrous metallurgy. SUBSTANCE: manganese mineral is first mixed with fired dolomite at ratio (CaO+1.4MgO)/Mn 9.5-1.0, whereupon is baked under oxidizing atmosphere to produce mix of manganite-maroquite concentrate which is further mixed with aluminium-silicon-manganese-iron alloy and a binder and briquetted. According to invention, mix of concentrate is baked in oxidizing atmosphere at 920-950 C for 1-2 h and obtained concentrate is cooled in the temperature range 920-680 C with rate 100-120 C/h. Method may be used for deoxidation and alloying of steel with manganese. EFFECT: increased yield of manganese and decreased hygroscopicity of briquets. 2 cl, 3 tbl
机译:领域:黑色冶金。物质:首先将锰矿物与烧成的白云石以(CaO + 1.4MgO)/ Mn 9.5-1.0的比例混合,然后在氧化气氛下烘烤,生成锰-马洛基铁精矿的混合物,然后将其与铝-硅-锰-铁进一步混合合金和粘合剂并压成团块。根据本发明,将浓缩物的混合物在氧化气氛中在920-950℃下烘烤1-2h,并将得到的浓缩物在920-680℃的温度范围内以100-120℃/ h的速率冷却。该方法可用于钢与锰的脱氧和合金化。效果:提高锰的产量,降低团块的吸湿性。 2厘升,3汤匙

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号