PURPOSE: To embody water penetrative pavement of high strength and large dry contractibility by means of easy site contruction by mixing a water penetrative pavement composition made of Portland cement or the like with water and kneading the mixture. ;CONSTITUTION: Composition for water penetrative pavement consisting of 300-400 pts.wt. Portland cement, 1400-1600 pts.wt. No.6 or 7 dry broken stone aggregate, 0.5-5 pts.wt. mixing agent powder for water-soluble or water dispersing cement is prepared. At the time of forming 1m3 water penetrative concrete, the composition for water penetrative pavement is mixed and kneaded with water so that a water cement ratio may become 30-40%, and then, construction is executed at a required place. By the way, as for this composition for water penetrative pavement, it is desirable that the adhesion water of the dry broken stone aggregate is less than 3wt.% in regard to that of the aggregate dried at 105°C. Also, it is desirable that more than 70wt.% of the mixing agent powder consists of polymer dispersion powder.;COPYRIGHT: (C)1994,JPO&Japio
机译:用途:通过将波特兰水泥等制成的水渗透性路面组合物与水混合并捏合,通过容易的现场施工来体现高强度和大干收缩性的水渗透性路面。 ;组成:透水路面的组成,由300-400 pts.wt.组成。波特兰水泥,1400-1600 pts.wt. 6-5号干碎石骨料,0.5-5 pts.wt.制备用于水溶性或水分散性水泥的混合剂粉末。在形成1m 3 渗水混凝土时,将渗水路面用组合物与水混合并捏合,使水灰比达到30-40%,然后在一个必需的地方。顺便提及,对于这种用于透水铺路的组合物,希望干燥的碎石骨料的粘附水相对于在105℃下干燥的骨料的粘附水小于3重量%。另外,希望混合剂粉末的70重量%以上由聚合物分散粉末组成。COPYRIGHT:(C)1994,JPO&Japio

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号