首页> 外国专利> Method for formulating three-wavelength fluorescent material and three- wavelength fluorescent lamp-using fluorescent material produced by the same

Method for formulating three-wavelength fluorescent material and three- wavelength fluorescent lamp-using fluorescent material produced by the same

机译:制备三波长荧光材料的方法和使用由其制备的三波长荧光灯的荧光材料

摘要

There is provided a method for formulating a three-wavelength fluorescent material 2 in which a blue fluorescent material B2 has a half- width value of 25 to 40 nm, a green fluorescent material has a particle diameter of 4.0 to 8.0 &mgr;m, and the blue florescent material B2/green fluorescent material G2/red fluorescent material R1 mixing ratio is 29. 2:42.0:28.8. The present invention makes it possible to improve the brightness of a three-wavelength florescent lamp 1 using this three- wavelength fluorescent material 2 by substantially 13% and the flux of light thereof by substantially 4%, thus realizing a brighter three- wavelength fluorescent lamp.
机译:提供了一种配制三波长荧光材料2的方法,其中蓝色荧光材料B2的半峰值为25-40nm,绿色荧光材料的粒径为4.0-8.0μm,并且蓝色荧光材料B2 /绿色荧光材料G2 /红色荧光材料R1的混合比为29。2:42.0:28.8。本发明使得使用这种三波长荧光材料2的三波长荧光灯1的亮度提高大约13%,并且其光通量提高大约4%,从而实现了更亮的三波长荧光灯。 。

著录项

  • 公开/公告号US5821687A

    专利类型

  • 公开/公告日1998-10-13

    原文格式PDF

  • 申请/专利权人 STANLEY ELECTRIC CO. LTD.;

    申请/专利号US19970797488

  • 发明设计人 MASAFUMI MIZUNO;HIROHISA MIYAZAKI;

    申请日1997-02-07

  • 分类号H01J1/62;

  • 国家 US

  • 入库时间 2022-08-22 02:38:22

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号