PROBLEM TO BE SOLVED: To provide a method for producing a material for civil engineering and construction out of a waste paper such as a newspaper, magazine and wrapping paper as a raw material because the recycling amount is only extremely small amount compared to that of the newspaper, magazine, etc., disposed of by homes, and the waste paper is in a state in which a large amount thereof is burned or subjected to a burying treatment under the ground nevertheless the recycling technique is established. ;SOLUTION: A muddy waste paper colloidal sediment formed by blending a waste paper with water in an amount of 10-30 times as much as the amount of the waste paper, and stirring the blend, is wrapped with a water-permeable sheet and inserted in a water-removing and forming frame and the obtained one or more naturally dewatered and laminated sheets are compulsory pressed and dewatered, or the muddy waste paper colloidal sediment is wrapped with the water-permeable sheet and allowed to be dewatered to loose 60-80% water. The dewatered material is blended with a vinyl acetate resin emulsion and kneaded, and the kneaded material is dewatered by subjecting the kneaded material to compulsory pressing by the forming and dewatering frame, or wrapping the kneaded material with the water- permeable sheet to be dewatered so as to loose 50-70% water. The dewatered product is blended and kneaded with a cement and the product is inserted into the dewatering and forming frame, formed and dried in the method for producing a material for civil engineering and construction out of a waste paper.;COPYRIGHT: (C)1999,JPO
机译:要解决的问题:提供一种方法,以废纸(例如报纸,杂志和包装纸)为原料,来生产用于土木工程和建筑业的材料,因为与之相比,其再循环量非常小。报纸,杂志等由家庭处置,并且废纸处于大量燃烧或在地下进行掩埋处理的状态,但是建立了回收技术。 ;解决方案:通过将废纸与废纸量的10-30倍量的水混合并搅拌,形成的浑浊废纸胶体沉淀物,然后用透水片包裹并插入在脱水成型机​​中,将获得的一层或多层自然脱水和层压的片材强制压榨或脱水,或将浑浊的废纸胶体沉淀物包裹在透水片材上,使其脱水以松散60-80 % 水。将脱水后的材料与乙酸乙烯酯树脂乳液混合并捏合,然后通过在成形和脱水框架中对捏合后的材料进行强制加压,或者将捏合后的材料用待透水的片材包裹,从而使捏合后的材料脱水。如洒水50-70%。将脱水后的产品与水泥混合并捏合,然后将产品插入脱水成型框架中,并按照废纸制造土木和建筑材料的方法进行成型和干燥。版权所有:(C)1999 ,日本特许厅

著录项

  • 公开/公告号JP3160604B2

    专利类型

  • 公开/公告日2001-04-25

    原文格式PDF

  • 申请/专利权人 村本 修;

    申请/专利号JP19970284222

  • 发明设计人 村本 修;

    申请日1997-09-09

  • 分类号D21J1/04;B09B3/00;

  • 国家 JP

  • 入库时间 2022-08-22 01:32:51

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号