PRODUCTION OF POLYETHERESTER ELASTIC FIBER HAVING EXCELLENT HEAT RESISTANCE

机译:具有出色耐热性的聚氨酯弹性纤维的生产

摘要

PURPOSE: A process for preparing the title fiber by synthesizing a polyetherester block copolymer and melt spinning is provided, which produces polyetherester elastic fiber having excellent heat resistance during dyeing and processing processes as well as excellent elastic recovery properties. CONSTITUTION: This polyetherester elastic fiber is prepared by using 20 to 40 parts by weight of 2,6-naphthalenecarboxylate as an acidic component of a hard segment component and a polyetherester block copolymer comprising polyoxyalkyleneglycol as a soft segment. The polyetherester block copolymer satisfies the following formula (1) 1.7 IV2.2, (2) Tm190deg.C, and (3) 2Mw/Mn4, wherein IV represents intrinsic viscosity, Tm is a melting point, Mw is a weight average molecular weight, and Mn is a number average molecular weight.
机译:目的:提供一种通过合成聚醚酯嵌段共聚物并熔融纺丝制备标题纤维的方法,该方法生产的聚醚酯弹性纤维在染色和加工过程中具有优异的耐热性以及优异的弹性回复性能。组成:该聚醚酯弹性纤维是通过使用20至40重量份的2,6-萘甲酸二乙酯作为硬链段组分的酸性组分和包含聚氧化烯二醇作为软链段的聚醚酯嵌段共聚物制成的。聚醚酯嵌段共聚物满足下式(1)1.7 IV2.2,(2)Tm190℃,和(3)2Mw / Mn4,其中IV表示特性粘度,Tm是熔点,Mw是重均分子量,并且Mn是数均分子量。

著录项

  • 公开/公告号KR20010029274A

    专利类型

  • 公开/公告日2001-04-06

    原文格式PDF

  • 申请/专利权人 HUVIS CORPORATION.;

    申请/专利号KR19990042014

  • 发明设计人 LEE MIN SEONG;

    申请日1999-09-30

  • 分类号D01F8/14;

  • 国家 KR

  • 入库时间 2022-08-22 01:13:53

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号